@article{oai:oist.repo.nii.ac.jp:00001875, author = {Li, Wenbo and Li, Zhaoning and Si, Changfeng and Wong, Michael Y. and Jinnai, Kazuya and Gupta, Abhishek Kumar and Kabe, Ryota and Adachi, Chihaya and Huang, Wei and Zysman‐Colman, Eli and Samuel, Ifor D. W.}, issue = {45}, journal = {Advanced Materials}, month = {Oct}, note = {Organic long-persistent luminescence (OLPL) is one of the most promising methods for long-lived-emission applications. However, present room-temperature OLPL emitters are mainly based on a bimolecular exciplex system which usually needs an expensive small molecule such as 2,8-bis(diphenyl-phosphoryl)dibenzo[b,d]thiophene (PPT) as the acceptor. In this study, a new thermally activated delayed fluorescence (TADF) compound, 3-(4-(9H-carbazol-9-yl)phenyl)acenaphtho[1,2-b]pyrazine-8,9-dicarbonitrile (CzPhAP), is designed, which also shows OLPL in many well-known hosts such as PPT, 2,2',2''-(1,3,5-benzinetriyl)-tris(1-phenyl-1-H-benzimidazole) (TPBi), and poly(methyl methacrylate) (PMMA), without any exciplex formation, and its OLPL duration reaches more than 1 h at room temperature. Combining the low cost of PMMA manufacture and flexible designs of TADF molecules, pure organic, large-scale, color tunable, and low-cost room-temperature OLPL applications become possible. Moreover, it is found that the onset of the 77 K afterglow spectra from a TADF-emitter-doped film is not necessarily reliable for determining the lowest triplet state energy level. This is because in some TADF-emitter-doped films, optical excitation can generate charges (electron and holes) that can later recombine to form singlet excitons during the phosphorescence spectrum measurement. The spectrum taken in the phosphorescence time window at low temperature may consequently consist of both singlet and triplet emission.}, title = {Organic Long‐Persistent Luminescence from a Thermally Activated Delayed Fluorescence Compound}, volume = {32}, year = {2020} }